Polymers

Group Short Name ↓ Name
HTRTP (HBA/HNA)-LCP Hydroxybenzoic acid-2,6- hydroxynaphthenic acid (liquid crystalline polymer)
CTP ABS Acrylonitrile-Butadiene-Styrene Copolymer
CTP ASA Acrylonitrile-styrene- acrylate copolymer
EM BR Butadiene rubber
EM CM Chlorinated polyethylene rubber
EM CR Chloroprene rubber
TS EP Epoxy resin
EM EPDM Ethylene-propylene-diene rubber
HTRTP ETFE Ethylene-tetrafluoroethylene
CTP EVA Polyethylene-co-vinyl acetate
HTRTP FEP Tetrafluoroethylene/hexafluoropropylene copolymer
EM HNBR Hydrogenated acrylonitrile-butadiene rubber
TS MF Melamine-formaldehyde resin
EM NBR Acrylonitrile-butadiene rubber
EM NR Natural rubber
ETP PA11 Polyamide 11
ETP PA12 Polyamide 12
ETP PA46 Polyamide 46
ETP PA6 Polyamide 6
HTRTP PA6/3T Polyamide 6/3T
HTRTP PA6/6T Polyamide 6/6T
ETP PA610 Polyamide 610
ETP PA612 Polyamide 612
ETP PA66 Polyamide 66
CTP PB Polybutene
ETP PBT Polybutylene terephthalate
ETP PC Polycarbonate
HTRTP PEEK Polyetheretherketone
CTP PE-HD Polyethylene high density
HTRTP PEI Polyetherimide
HTRTP PEKEKK Polyacryletherketone- etherketoneketone
CTP PE-LD Polyethylene low density
CTP PE-LLD Polyethylene linear low density
HTRTP PES Polyethersulfone
ETP PET Polyethylene terephthalate
CTP PE-UHMW Polyethylene ultra high molecular weight
TS PF Phenol-formaldehyde resin
HTRTP PFA Perfluoroalkoxy
CTP PIB Polyisobutylene
CTP PLA Polylactide
ETP PMMA Polymethylmethacrylate
ETP POM (copo) Polyoxymethylene (copolymer)
ETP POM (homo) Polyoxymethylene (homopolymer)
CTP PP (isotactic) Polypropylene
HTRTP PPS Polyphenylenesulfide
CTP PS Polystyrene
HTRTP PSU Polysulfone
HTRTP PTFE Polytetrafluoroethylene
TS PUR Polyurethane
CTP PVAL Polyvinylalcohol
CTP PVC-P Polyvinylchloride (with plasticizer)
CTP PVC-U Polyvinylchloride (without plasticizer)
CTP PVDC Polyvinylidene chloride
HTRTP PVDF Polyvinylidene fluoride
HTRTP PVF Polyvinylfluoride
EM Q Silicone rubber
CTP SAN Styrene-acrylonitrile copolymer
CTP SB Styrene/Polybutadiene copolymer
EM SBR Styrene-butadiene rubber
TPEM TPA Amide based TPE
TPEM TPC Ester-Ether based TPE
TPEM TPO, TPV Polyolefine based TPE
TPEM TPS Styrene based TPE
TPEM TPU Urethane based TPE
TS UF Urea-formaldehyde resin
TS UP Unsaturated polyester resin