Coefficient of Linear Thermal Expansion
Description
Coefficient of Linear Thermal Expansion (CLTE) is the change in length per unit length of a material per degree of temperature change.
Dilatometry (DIL)
Dilatometry (DIL) is a thermoanalytical technique for the measurement of expansion or shrinking of a polymeric material with subjected to a controlled temperature/time program.