PVDC: Polyvinylidene chloride


Short Name
PVDC
Name
Polyvinylidene chloride
Group
CTP - Commodity Thermoplastics
General Properties
Chemical Formula
Structural Formula

Properties

Glass Transition Temperature
-18 to +15 °C
Melting Temperature
140 to 210 °C
Melting Enthalpy
(na) J/g
Decomposition Temperature
245 to 255 °C
Young's Modulus
300 to 550 MPa
Coefficient of Linear Thermal Expansion
190 *10¯6/K
Specific Heat Capacity
(na) J/(g*K)
Thermal Conductivity
0.13 W/(m*K)
Density
1.63 g/cm³