(HBA/HNA)-LCP: Hydroxybenzoic acid-2,6- hydroxynaphthenic acid (liquid crystalline polymer)
-
Short Name
-
(HBA/HNA)-LCP
-
Name
-
Hydroxybenzoic acid-2,6- hydroxynaphthenic acid (liquid crystalline polymer)
-
Group
-
HTRTP
- High-Temperature Resistant Thermoplastics
-
General Properties
-
-
Chemical Formula
-
- Structural Formula
-
NETZSCH Measurements