CTP Commodity Thermoplastics


Group Name ↓ Short Name Name Formula
CTP ABS Acrylonitrile-Butadiene-Styrene Copolymer (C8H8)n1 (C4H6)n2 (C3H3N)n3
CTP ASA Acrylonitrile-styrene- acrylate copolymer
CTP EVA Polyethylene-co-vinyl acetate (C2H4)n(C4H6O2)m
CTP PB Polybutene
CTP PE-HD Polyethylene high density
CTP PE-LD Polyethylene low density
CTP PE-LLD Polyethylene linear low density
CTP PE-UHMW Polyethylene ultra high molecular weight
CTP PIB Polyisobutylene
CTP PLA Polylactide
CTP PP (isotactic) Polypropylene (C3H6)n
CTP PS Polystyrene (C8H8)n
CTP PVAL Polyvinylalcohol
CTP PVC-P Polyvinylchloride (with plasticizer)
CTP PVC-U Polyvinylchloride (without plasticizer)
CTP PVDC Polyvinylidene chloride
CTP SAN Styrene-acrylonitrile copolymer
CTP SB Styrene/Polybutadiene copolymer